Joggle lap shear testing of deep occlusal composite restorations lined with Dycal, Dycal LC, conventional or resin-modified glass ionomer

Stojanovska, Vera; Ivanoff, Chris S.; Muratovska, Ilijana; Popovska, Lidija; Garcia-Godoy, Franklin; Hottel, Timothy L.; Marković, Dejan; Morrow, Brian R.

(Vojnomedicinska akademija - Institut za naučne informacije, Beograd, 2017)

TY  - JOUR
AU  - Stojanovska, Vera
AU  - Ivanoff, Chris S.
AU  - Muratovska, Ilijana
AU  - Popovska, Lidija
AU  - Garcia-Godoy, Franklin
AU  - Hottel, Timothy L.
AU  - Marković, Dejan
AU  - Morrow, Brian R.
PY  - 2017
UR  - https://smile.stomf.bg.ac.rs/handle/123456789/2238
AB  - Background/Aim. The longevity of a dental restoration may be predicted to some degree by its adhesive ability, and this, in turn, can be measured by bond strength testing between restorative materials and tooth structure. The aim of this study was to test an innovative joggle lap shearing jig that integrates the tooth and the entire biomechanical unit into testing, to compare the shear bond strengths of Class I occlusal composite restorations in deep cavity preparations lined with Dycal, Dycal LC, conventional glass ionomer or resin-modified glass ionomer. The mode of failure (adhesive, cohesive, mixed) after debonding was determined by stereomicroscopy. Methods. A total of 150 standardized occlusal cavities were prepared and divided into five groups. The group I cavities (n = 30) were coated with adhesive (ExciTE®F) and filled directly with composite (TetricEvoCeram). The group II and III cavities were lined with Dycal (n = 30) or Dycal LC (n = 30) before placing composite. The groups IV and V specimens were based with Fuji IX (n = 30) or Fuji II LC (n = 30). Shear bond strengths were determined with a universal testing machine and fractured bonding sites were analyzed under stereomicroscope. The mean bond strengths were analyzed using one-way ANOVA test (p  lt  0.05) and the means between the groups were analyzed with Student's t-test. Results. The shear bond strength (MPa) of composite restorations in cavities without base (23.91 ± 4.54) was higher than cavities lined with Fuji II LC (17.45 ± 2.74), Fuji IX (8.76 ± 2.57), Dycal LC (13.07 ± 1.84) or Dycal (6.12 ± 1.28). The results using the jogged lap shearing jig were consistent with the literature. Conclusion. The shear bond strength of occlusal composite restorations in deep cavities without liners was greater than cavities lined with Fuji II LC > Fuji IX > Dycal LC > Dycal.
AB  - Uvod/Cilj. Trajnost zubnih nadoknada može se donekle predvideti vstom adhezivne sposobnosti materijala i može se meriti testiranjem snage adhezije restorativnih materijala i zubnih struktura. Cilj ove studije bio je da se da se testira preklapanje spoja koji povezuje zub i biomehaničku jedinicu i da se uporedi jačina veze okluzalnih kompozitnih ispuna postavljenih u duboke kavitete preko podloge od Dycal, Dycal LC, konvencionalnog ili smolom-modifikovanog glas-jonomer cementa. Metode. Ukupno 150 standardizovanih okluzalnih kaviteta bilo je podeljeno u pet grupa (n = 30): I - kaviteti premazani adhezivom (ExciTE®F) i direktno ispunjeni kompozitom (TetricEvoCeram); II i III - kaviteti sa podlogom od Dycal ili Dycal LC pre postavljanja kompozitnog materijala; IV i V - uzorci sa bazom od Fuji IX ili Fuji II LC (n = 30). Jačina vezivne snage određena je pomoću univerzalne mašine, a način neuspeha (adhezivna, kohezivna, mešovita fraktura) određen je stereomikroskopom. Srednje vrednosti su analizirane pomoću ANOVA testa (p  lt  0,05), a značajnost razlika između grupa analizirana je Student-ovim t-testom. Rezultati. Jačina vezivne snage (MPa) kompozitnih ispuna u kavitetima bez podloge (23,91 ± 4,54) bila je veća u poređenju sa ispunima postavljenim preko Fuji II LC (17,45 ± 2,74), Fuji IX (8,76 ± 2,57), Dycal LC (13,07 ± 1,84) ili Dycal (6.12 ± 1.28). Zaključak. Smicanje ili pomaknuće okluzalnih kompozitnih ispuna u dubokim kavitetima bez lajnera je veće nego u kavitetima postavljenim preko Fuji II LC > Fuji IX > Dycal LC > Dycal.
PB  - Vojnomedicinska akademija - Institut za naučne informacije, Beograd
T2  - Vojnosanitetski pregled
T1  - Joggle lap shear testing of deep occlusal composite restorations lined with Dycal, Dycal LC, conventional or resin-modified glass ionomer
T1  - Testiranje spojnog smicanja dubokih okluzalnih kompozitnih restauracija postavljenih preko podloge od Dycal, Dycal LC, konvencionalnog ili smolom modifikovanog glas-jonomer cementa
VL  - 74
IS  - 5
SP  - 410
EP  - 419
DO  - 10.2298/VSP150816226S
ER  - 
@article{
author = "Stojanovska, Vera and Ivanoff, Chris S. and Muratovska, Ilijana and Popovska, Lidija and Garcia-Godoy, Franklin and Hottel, Timothy L. and Marković, Dejan and Morrow, Brian R.",
year = "2017",
abstract = "Background/Aim. The longevity of a dental restoration may be predicted to some degree by its adhesive ability, and this, in turn, can be measured by bond strength testing between restorative materials and tooth structure. The aim of this study was to test an innovative joggle lap shearing jig that integrates the tooth and the entire biomechanical unit into testing, to compare the shear bond strengths of Class I occlusal composite restorations in deep cavity preparations lined with Dycal, Dycal LC, conventional glass ionomer or resin-modified glass ionomer. The mode of failure (adhesive, cohesive, mixed) after debonding was determined by stereomicroscopy. Methods. A total of 150 standardized occlusal cavities were prepared and divided into five groups. The group I cavities (n = 30) were coated with adhesive (ExciTE®F) and filled directly with composite (TetricEvoCeram). The group II and III cavities were lined with Dycal (n = 30) or Dycal LC (n = 30) before placing composite. The groups IV and V specimens were based with Fuji IX (n = 30) or Fuji II LC (n = 30). Shear bond strengths were determined with a universal testing machine and fractured bonding sites were analyzed under stereomicroscope. The mean bond strengths were analyzed using one-way ANOVA test (p  lt  0.05) and the means between the groups were analyzed with Student's t-test. Results. The shear bond strength (MPa) of composite restorations in cavities without base (23.91 ± 4.54) was higher than cavities lined with Fuji II LC (17.45 ± 2.74), Fuji IX (8.76 ± 2.57), Dycal LC (13.07 ± 1.84) or Dycal (6.12 ± 1.28). The results using the jogged lap shearing jig were consistent with the literature. Conclusion. The shear bond strength of occlusal composite restorations in deep cavities without liners was greater than cavities lined with Fuji II LC > Fuji IX > Dycal LC > Dycal., Uvod/Cilj. Trajnost zubnih nadoknada može se donekle predvideti vstom adhezivne sposobnosti materijala i može se meriti testiranjem snage adhezije restorativnih materijala i zubnih struktura. Cilj ove studije bio je da se da se testira preklapanje spoja koji povezuje zub i biomehaničku jedinicu i da se uporedi jačina veze okluzalnih kompozitnih ispuna postavljenih u duboke kavitete preko podloge od Dycal, Dycal LC, konvencionalnog ili smolom-modifikovanog glas-jonomer cementa. Metode. Ukupno 150 standardizovanih okluzalnih kaviteta bilo je podeljeno u pet grupa (n = 30): I - kaviteti premazani adhezivom (ExciTE®F) i direktno ispunjeni kompozitom (TetricEvoCeram); II i III - kaviteti sa podlogom od Dycal ili Dycal LC pre postavljanja kompozitnog materijala; IV i V - uzorci sa bazom od Fuji IX ili Fuji II LC (n = 30). Jačina vezivne snage određena je pomoću univerzalne mašine, a način neuspeha (adhezivna, kohezivna, mešovita fraktura) određen je stereomikroskopom. Srednje vrednosti su analizirane pomoću ANOVA testa (p  lt  0,05), a značajnost razlika između grupa analizirana je Student-ovim t-testom. Rezultati. Jačina vezivne snage (MPa) kompozitnih ispuna u kavitetima bez podloge (23,91 ± 4,54) bila je veća u poređenju sa ispunima postavljenim preko Fuji II LC (17,45 ± 2,74), Fuji IX (8,76 ± 2,57), Dycal LC (13,07 ± 1,84) ili Dycal (6.12 ± 1.28). Zaključak. Smicanje ili pomaknuće okluzalnih kompozitnih ispuna u dubokim kavitetima bez lajnera je veće nego u kavitetima postavljenim preko Fuji II LC > Fuji IX > Dycal LC > Dycal.",
publisher = "Vojnomedicinska akademija - Institut za naučne informacije, Beograd",
journal = "Vojnosanitetski pregled",
title = "Joggle lap shear testing of deep occlusal composite restorations lined with Dycal, Dycal LC, conventional or resin-modified glass ionomer, Testiranje spojnog smicanja dubokih okluzalnih kompozitnih restauracija postavljenih preko podloge od Dycal, Dycal LC, konvencionalnog ili smolom modifikovanog glas-jonomer cementa",
volume = "74",
number = "5",
pages = "410-419",
doi = "10.2298/VSP150816226S"
}
Stojanovska, V., Ivanoff, C. S., Muratovska, I., Popovska, L., Garcia-Godoy, F., Hottel, T. L., Marković, D.,& Morrow, B. R.. (2017). Joggle lap shear testing of deep occlusal composite restorations lined with Dycal, Dycal LC, conventional or resin-modified glass ionomer. in Vojnosanitetski pregled
Vojnomedicinska akademija - Institut za naučne informacije, Beograd., 74(5), 410-419.
https://doi.org/10.2298/VSP150816226S
Stojanovska V, Ivanoff CS, Muratovska I, Popovska L, Garcia-Godoy F, Hottel TL, Marković D, Morrow BR. Joggle lap shear testing of deep occlusal composite restorations lined with Dycal, Dycal LC, conventional or resin-modified glass ionomer. in Vojnosanitetski pregled. 2017;74(5):410-419.
doi:10.2298/VSP150816226S .
Stojanovska, Vera, Ivanoff, Chris S., Muratovska, Ilijana, Popovska, Lidija, Garcia-Godoy, Franklin, Hottel, Timothy L., Marković, Dejan, Morrow, Brian R., "Joggle lap shear testing of deep occlusal composite restorations lined with Dycal, Dycal LC, conventional or resin-modified glass ionomer" in Vojnosanitetski pregled, 74, no. 5 (2017):410-419,
https://doi.org/10.2298/VSP150816226S . .
2
1
1