@article{
author = "Miletić, Vesna and Santini, Ario",
year = "2012",
abstract = "The aim of this study was to optimize the concentration of 2,4,6-trimethylbenzoyldiphenylphosphine oxide (Lucirin (R) TPO) in unfilled and filled composite resins in relation to the degree of conversion (DC). Increasing concentrations of Lucirin (R) TPO between 0.05-4.97 wt% were added to equimolar mixtures of Bis-GMA/TEGDMA. Filled resins contained 75 wt% fillers. Standardized samples were cured using a polywave LED light-curing unit (bluephase (R) G2, Ivoclar Vivadent). Increased initiator concentrations increased logarithmically the DC of unfilled and filled resins. The DC of unfilled resins was in the range of 73-91% at the top and 63-81% at the bottom surfaces and that of filled resins was in the range of 53-81% at the top and 47-70% at the bottom surfaces. The DC in unfilled and filled resins reached a plateau at 1.08 wt% and 1.50 wt% Lucirin (R) TPO, respectively. Fillers significantly reduced conversion but had no effect on the logarithmic relationship between initiator concentration and the DC.",
publisher = "Japanese Soc Dental Materials Devices, Tokyo",
journal = "Dental Materials Journal",
title = "Optimizing the concentration of 2,4,6-trimethylbenzoyldiphenylphosphine oxide initiator in composite resins in relation to monomer conversion",
volume = "31",
number = "5",
pages = "717-723",
doi = "10.4012/dmj.2012-064"
}