Challenges in experimental evaluation of morphological, chemo-mechanical and adhesive properties of glass-ionomer based dental materials
(Advanced Technologies & Materials, 2019)
Changes in composition and new material characteristics require verification in clinical and experimental studies. Investigating glass-ionomer cements under laboratory conditions encounters problems in interpreting the ...