dc.description.abstractObjectives: To determine the extent of the hybrid layer (HL) of the novel adhesive system (Silorane, 3M ESPE) compared to one-step and etch and rinse adhesive systems, using 2D confocal micro-Roman spectroscopy and SEM. Methods: Silorane adhesive system was compared to two one-step self-etch (G Bond, GC; AdheSE One, Ivoclar Vivadent) and etch and rinse (Excite, Ivoclar Vivadent) as controls. Adhesives were applied to human dentine, cured and sections prepared perpendicular to the flat adhesive-dentine surface. Two-dimensional micro-Roman mapping was performed over 20 mu m x 20 mu m areas across the adhesive-dentine interface. SEM micrographs of the same specimens were obtained. One-way ANOVA (Tukey's post-test) was used to analyse the differences in HL thickness among the four adhesive systems and the paired t-test to compare the results obtained by micro-Roman and SEM for each adhesive. Results: Silorane adhesive system formed a HL of comparable thickness to methacrylate-based but thicker than the acrylamide-based one-step self-etch adhesives from SEM analysis. A gradual decrease in adhesive penetration was observed in all systems. A 1-mu m zone, between the cured primer and bond was identified by Raman but not visualised on SEM. Compared to SEM, HL calculated from Raman data were always greater. Conclusions: Micro-Roman spectroscopy gives a more precise indication of dentine demineralisation and monomer infiltration and highlights the intermediate zone of similar to 1 mu m between Silorane primer and bond, not visible with SEM at x10,000 magnification. Giving as it does, a compilation of many linear scans it allows HL mean values to be calculated.en
dc.publisherElsevier Sci Ltd, Oxford
dc.rightsrestrictedAccess
dc.sourceJournal of Dentistry
dc.subjectconfocal micro-Ramanen
dc.subjectspectroscopyen
dc.subjectSEMen
dc.subjecthybrid layeren
dc.subjectself-etch adhesivesen
dc.titleComparison of the hybrid layer formed by Silorane adhesive, one-step self-etch and etch and rinse systems using confocal micro-Raman spectroscopy and SEMen
dc.typearticle
dc.rights.licenseARR
dcterms.abstractМилетић, Весна; Сантини, Aрио;
dc.citation.volume36
dc.citation.issue9
dc.citation.spage683
dc.citation.epage691
dc.citation.other36(9): 683-691
dc.citation.rankM21
dc.identifier.wos000259659200003
dc.identifier.doi10.1016/j.jdent.2008.04.016
dc.identifier.pmid18550251
dc.identifier.scopus2-s2.0-48549087606
dc.type.versionpublishedVersion


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу