dc.description.abstractObjectives: To quantify monomer elution from different adhesive systems using reverse-phase high-performance liquid chromatography (HPLC) and correlate this elution with the ratio of carbon-carbon double bonds from monomer to polymer (RDB) obtained using micro-Raman spectroscopy. Methods: Thirty dentine discs were cut from 30 human, intact, third molars and randomly allocated to five groups according to the adhesive applied: total-etch, Excite (Ivoclar Vivadent), two-bottle self-etch, Clearfil SE (Kuraray), one-bottle self-etch, Clear-fil 3S (Kuraray), ormocer-based, Admira (Voco) and Filtek Silorane adhesive system (FS) (3M ESPE). Monomer elution was studied 1 h, 6 h, 24 h, 96 h and 7 days after immersion in 75% ethanol/water. The RDB was calculated immediately after light-curing and thereafter at 24 h and 7 days. The data were statistically analysed using one-way ANOVA and Pearson's correlation coefficient (p lt 0.05). Results: More than 90% of the whole elution occurred during the first I h, except for BisGMA in FS, with the highest absolute amount from Clearfil SE and the highest wt% from Admira. initial RDB was in the ascending order FS lt Admira lt Excite lt Clearfil SE lt Clearfil 3S. in all groups, the RDB was significantly higher after 24 h and 7 days than immediately after light-curing (p lt 0.05). Negative correlation was found only for the elution of HEMA and the RDB of Clearfil 3S. Conclusions: Different adhesive systems showed different monomer elution kinetics. In all systems, the RDB increased after monomer elution. Overall, no direct correlation exists between the RDB of adhesives and the elution of unreacted monomers.en
dc.publisherElsevier Sci Ltd, Oxford
dc.rightsrestrictedAccess
dc.sourceJournal of Dentistry
dc.subjectAdhesiveen
dc.subjectMonomeren
dc.subjectElutionen
dc.subjectHPLCen
dc.subjectDegree of conversionen
dc.subjectRamanen
dc.subjectDimethacrylateen
dc.subjectOrmoceren
dc.subjectSiloraneen
dc.titleQuantification of monomer elution and carbon-carbon double bonds in dental adhesive systems using HPLC and micro-Raman spectroscopyen
dc.typearticle
dc.rights.licenseARR
dcterms.abstractМилетић, Весна; Тркуља, Иван; Сантини, Aрио;
dc.citation.volume37
dc.citation.issue3
dc.citation.spage177
dc.citation.epage184
dc.citation.other37(3): 177-184
dc.citation.rankM21
dc.identifier.wos000263442900002
dc.identifier.doi10.1016/j.jdent.2008.11.006
dc.identifier.pmid19108941
dc.identifier.scopus2-s2.0-58249129300
dc.type.versionpublishedVersion


Dokumenti

Thumbnail

Ovaj dokument se pojavljuje u sledećim kolekcijama

Prikaz osnovnih podataka o dokumentu