dc.description.abstractPurpose: To evaluate the microleakage of Class II cavities restored with experimental low-shrinking resin composites proposed for bulk filling and to measure their microtensile bond strength (mu TBS) to dentin and compare to those of previously marketed low-shrinkage composites. Methods: Class II cavities (7 mm occluso-gingival height, 2 mm mesio-distal depth of the box, 4 mm occlusal depth, 4 mm bucco-lingual width) were prepared in 50 molars and randomly divided into five groups (n=10), according to the material: SureFil SDR flow (SDR), Filtek Silorane (FS) and experimental materials (G-aenial Flo bulk fill, GF; G-aenial Universal Flo bulk fill, GUF; GC Kalore bulk fill, GK). Microleakage was separately assessed at enamel and dentin margins by scoring the depth of silver-nitrate penetration. Twenty teeth divided into five groups (n= 4) were selected for mu TBS testing. The same materials as for microleakage assessment were placed in bulk to mid-coronal dentin. Microtensile beams were loaded in tension, and mu TBS at failure was calculated in MPa. Microleakage and mu TBS data were analyzed by ANOVA on ranks, followed Dunn's post hoc test (P lt 0.05). Results: Microleakage was not observed at the enamel interface in any of the groups. At the dentin interface, SDR recorded significantly higher microleakage than the other materials. mu TBS of GF, GUF and GK did not differ among each other (33 +/- 12 MPa, 31 +/- 11 MPa, 30 +/- 9 MPa, respectively), while SDR (63 +/- 17 MPa) and FS (55 +/- 17MPa) achieved significantly higher mu TBS values. No direct association between the sealing properties and the bond strength values was observed.en
dc.rightsrestrictedAccess
dc.sourceAmerican Journal of Dentistry
dc.titleMicroleakage of Class II restorations and microtensile bond strength to dentin of low-shrinkage compositesen
dc.typearticle
dc.rights.licenseARR
dcterms.abstractВицхи, Aлессандро; Феррари, Марцо; Форнер, Леополдо; Царрабба, Мицхеле; Мануел Aрагонесес, Јуан; Јулоски, Јелена;
dc.citation.volume26
dc.citation.issue5
dc.citation.spage271
dc.citation.epage277
dc.citation.other26(5): 271-277
dc.citation.rankM23
dc.identifier.wos000326905700007
dc.identifier.scopus2-s2.0-84889874175
dc.identifier.rcubhttps://hdl.handle.net/21.15107/rcub_smile_1820
dc.type.versionpublishedVersion


Документи

ДатотекеВеличинаФорматПреглед

Уз овај запис нема датотека.

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу